In stress relief annealing, steel is heated to a temperature between ______

Nguyễn Trà

New member
In stress relief annealing, steel is heated to a temperature between ______
A. 200⁰C to 250⁰C
B. 300⁰C to 325⁰C
C. 385⁰C to 440⁰C
D. 500⁰C to 550⁰C
 
Answer: d
Explanation: Stress relief annealing process consists of three steps. In the first step, the cold worked steel is heated to a temperature between 500⁰C to 550⁰C i.e., below recrystallization temperature. The second step involves holding the steel component at this temperature for1-2 hours. The final step is to cool the steel component to room temperature in air.
 