Slow cooling of hypereutectoid steel results in formation of __________
A. Proeutectoid cementite
B. Posteutectoid cementite
C. Proeutectoid ferrite
D. Proeutectoid austenite
Answer: a
Explanation: Over 0.8% carbon steel is heated at around 925$^{o}$C and held at this temperature. This results in the formation of austenite. Then the steel is slowly cooled to form proeutectoid cementite which will nucleate and grow at austenite grain boundaries.