Hardness readings are taken every ________ after quenching in Jominy end-quench test.

Hardness readings are taken every ________ after quenching in Jominy end-quench test.
A. 0.01 mm
B. 0.1 mm
C. 1.6 mm
D. 2.5 mm
 
Answer: c
Explanation: The given sample of material is heated above the upper critical temperature. It is then quenched at one end at 25$^{o}$C. After cooling, a flat is ground along the length of the bar. Rockwell C hardness readings are then taken for every 1.6 mm along the length from the quenched end, which are then plotted in the form of a graph.
 