Numerous failures of 18-8 Stainless steel have occurred in the temperature range of 950 to 1450°F

Thành Nguyễn

New member
Numerous failures of 18-8 Stainless steel have occurred in the temperature range of 950 to 1450°F
A. True
B. False
 
Answer: a
Explanation: Numerous failures of 18-8 stainless steel have occurred in the temperature range of 950 to 1450°F. When these steels are heated in the range of 950 to 1450°F they become sensitized or susceptible to intergranular corrosion due to the depletion of chromium at the grain boundary.
 